Bu öğeden alıntı yapmak, öğeye bağlanmak için bu tanımlayıcıyı kullanınız:
http://hdl.handle.net/11452/28878
Tüm üstveri kaydı
Dublin Core Alanı | Değer | Dil |
---|---|---|
dc.contributor.author | Hurst, Roger C. | - |
dc.contributor.author | Turba, Krystof | - |
dc.contributor.author | Hähner, Peter | - |
dc.date.accessioned | 2022-09-29T07:36:13Z | - |
dc.date.available | 2022-09-29T07:36:13Z | - |
dc.date.issued | 2013 | - |
dc.identifier.citation | Gülçimen, B. vd. (2013). "Mechanical characterisation of a P91 weldment by means of small punch fracture testing". International Journal of Pressure Vessels and Piping, 105, 28-35. | en_US |
dc.identifier.issn | 0308-0161 | - |
dc.identifier.issn | 1879-3541 | - |
dc.identifier.uri | https://doi.org/10.1016/j.ijpvp.2013.02.005 | - |
dc.identifier.uri | https://www.sciencedirect.com/science/article/pii/S0308016113000240 | - |
dc.identifier.uri | http://hdl.handle.net/11452/28878 | - |
dc.description.abstract | Small Punch fracture tests were carried out in order to determine low temperature mechanical behaviour of a P91 steel weldment: weld metal, base metal, Heat Affected Zone-Fine Grained and Heat Affected Zone-Coarse Grained. The Heat Affected Zone-Fine Grained showed superior tensile properties in terms of displacement at fracture (ductility) and strength (maximum force) compared to the other zones, which became more pronounced at lower temperatures, whilst the weld metal exhibited inferior behaviour. Ductile Brittle Transition Temperatures were evaluated from Small Punch results for all zones and the results of base metal and weld metal were correlated with the transition temperatures obtained from Charpy V notch tests according to the CEN Code of Practice for Small Punch testing. Heat Affected Zone-Fine Grained with its finest structure exhibited the lowest transition temperature and the weld metal the highest. Heat Affected Zone-Coarse Grained and base metal were found to have quite similar transition temperature values. | en_US |
dc.language.iso | en | en_US |
dc.publisher | Elsevier | en_US |
dc.rights | info:eu-repo/semantics/closedAccess | en_US |
dc.subject | Engineering | en_US |
dc.subject | Small punch testing technique | en_US |
dc.subject | Fracture | en_US |
dc.subject | Charpy test | en_US |
dc.subject | P91 steel | en_US |
dc.subject | Ductile to brittle transition temperature | en_US |
dc.subject | Temper embrittlement | en_US |
dc.subject | Yield strength | en_US |
dc.subject | Welded-joint | en_US |
dc.subject | Creep test | en_US |
dc.subject | Steels | en_US |
dc.subject | Specimen | en_US |
dc.subject | Fracture | en_US |
dc.subject | Fracture testing | en_US |
dc.subject | Heat affected zone | en_US |
dc.subject | Charpy tests | en_US |
dc.subject | Charpy V-notch test | en_US |
dc.subject | Ductile-brittle transition temperature | en_US |
dc.subject | Ductile-to-brittle transition temperature | en_US |
dc.subject | Mechanical behaviour | en_US |
dc.subject | Mechanical characterisation | en_US |
dc.subject | P91 steel | en_US |
dc.subject | Small punch testing | en_US |
dc.subject | Temperature | en_US |
dc.title | Mechanical characterisation of a P91 weldment by means of small punch fracture testing | en_US |
dc.type | Article | en_US |
dc.identifier.wos | 000318667200004 | tr_TR |
dc.identifier.scopus | 2-s2.0-84876727716 | tr_TR |
dc.relation.tubitak | 2214 | tr_TR |
dc.relation.publicationcategory | Makale - Uluslararası Hakemli Dergi | tr_TR |
dc.contributor.department | Uludağ Üniversitesi/Mühendislik Fakültesi/Makine Mühendisliği Bölümü. | tr_TR |
dc.identifier.startpage | 28 | tr_TR |
dc.identifier.endpage | 35 | tr_TR |
dc.identifier.volume | 105 | tr_TR |
dc.relation.journal | International Journal of Pressure Vessels and Piping | en_US |
dc.contributor.buuauthor | Çakan, Betül Gülçimen | - |
dc.contributor.buuauthor | Durmuş, Ali | - |
dc.contributor.buuauthor | Ülkü, Sedat | - |
dc.relation.collaboration | Yurt dışı | tr_TR |
dc.relation.collaboration | Sanayi | tr_TR |
dc.subject.wos | Engineering, multidisciplinary | en_US |
dc.subject.wos | Engineering, mechanical | en_US |
dc.indexed.wos | SCIE | en_US |
dc.indexed.scopus | Scopus | en_US |
dc.wos.quartile | Q2 | en_US |
dc.contributor.scopusid | 36983839100 | tr_TR |
dc.contributor.scopusid | 55964532400 | tr_TR |
dc.contributor.scopusid | 6701921191 | tr_TR |
dc.subject.scopus | Punches; Creep; Indentation | en_US |
Koleksiyonlarda Görünür: | Scopus Web of Science |
Bu öğenin dosyaları:
Bu öğeyle ilişkili dosya bulunmamaktadır.
DSpace'deki bütün öğeler, aksi belirtilmedikçe, tüm hakları saklı tutulmak şartıyla telif hakkı ile korunmaktadır.