Title: Growth of binary Ni-Fe films: Characterisations at low and high potential levels
Authors: Kuru, Hilal
Koçkar, Hakan
Karaağaç, Oznur
Uludağ Üniversitesi/Fen-Edebiyat Fakültesi/Fizik Bölümü.
0000-0001-8220-6851
Alper, Mürsel
AAG-8795-2021
7005719283
Keywords: Materials science
Physics
Ni-Fe films
Electrodeposition
Anisotropic magnetoresistance
Magnetic properties
Structural analysis
Vacuum coating plant
Magnetic-properties
Anisotropic magnetoresistance
Deposition parameters
Nickel-iron
Wave-forms
Thin-films
Electrodeposition
Alloys
PH
High potential
Issue Date: 1-Mar-2015
Publisher: Elsevier
Citation: Kuru, H. vd. (2015). "Growth of binary Ni-Fe films: Characterisations at low and high potential levels". Journal of Magnetism and Magnetic Materials, 377, 59-64.
Abstract: Binary Ni-Fe films relating their magnetoresistance and magnetic properties with crystal structure and surface morphology, and the Corresponding film composition were investigated at low and high deposition potentials. Based on the results obtained horn a cyclic voltammetry curve, a potential region between -1.3 V and -1.8 V was selected, and the current-time transients were recorded to control the proper film growth. The Ni-Fe films were potentiostatically electrodeposited on polycrystalline titanium substrates at low (-1.3 V) and high (-1.8 V) deposition potential. The data from the energy dispersive X-ray spectrometry and the inductively coupled plasma atomic emission spectroscopy demonstrated that the Ni and Fe content in the films varied as the potential changed. The magnetotransport properties and magnetic characteristics studied by a vibrating sample magnetometer (VSM) were observed to be affected by the deposition potentials. All films were also noted to exhibit anisotropic magnetoresistance behaviour. At low potential, the magnitude of the longitudinal magnetoresistance (LMR) was high (3.93%) and that of the transverse magnetoresistance (TMR) was low (3.49%) while for the film at high potential the LMR (2.76%) and the TMR (3.66%) magnitudes were obtained. Magnetization measurements by VSM revealed that the saturation magnetization, M-s was 779 emu/cm(3) and saturation field, H-s was 142 Oe at low potential while for the films deposited at high potential the M-s and H-s were 749 emu/cm(3) and 262 Oe, respectively. However, the coercivities in the films were found to be around 4.5 Oe, regardless of the potential. Also, the magnetic easy axis was found to be in the film plane for all samples. The structural analysis of the films was carried out using the X-ray diffraction (XRD) and scanning electron microscopy (SEM) techniques. To XRD analysis, all films have a strong (111) texture of face-centred cubic structure and the lattice parameters, d-spacings and average grain size slightly changed with deposition potential. The films studied by SEM revealed that they have smaller grains grown at low deposition potential compared to those deposited at high potential. The differences observed in the properties of the films might be attributed to the compositional changes caused by the deposition potential.
URI: https://doi.org/10.1016/j.jmmm.2014.10.058
https://www.sciencedirect.com/science/article/pii/S030488531400969X
http://hdl.handle.net/11452/34252
ISSN: 0304-8853
Appears in Collections:Scopus
Web of Science

Files in This Item:
There are no files associated with this item.


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.