Başlık: | Removal of heavy-metal ions by magnetic beads containing triazole chelating groups |
Yazarlar: | Uzun, Lokman Yılmaz, Erkut Denizli, Adil Uludağ Üniversitesi/Fen-Edebiyat Fakültesi/Kimya Bölümü. Kara, Ali Osman, Bilgen Beşirli, Necati AAG-6271-2019 7102824859 15221651200 6507924888 |
Anahtar kelimeler: | Adsorption Conjugated polymers Gels Magnetic polymers Stabilized fluidized-bed Solid-phase extraction Antibody removal Adsorption Water Preconcentration Purification Mercury(ıı) Hydrogel Sorbents Polymer science Adsorption Conjugated polymers Ethylene Ethylene glycol Gelation Lead Iron ores Magnetic fields Mercury (metal) Metal ions Metal recovery Nitrogen compounds Oxide minerals Polymers Sewage Trace analysis Wastewater Zinc 1 ,2 ,4-Triazole Aquous solutions Binding capacities Chelating groups Ethylene glycol dimethacrylate Magnetic beads Magnetic polymers Metal removal Nano powders Suspension polymerization Swelling ratio Synthetic solutions Synthetic waste water Bead Magnet Polyethylene glycol Polymer solution Surface property Swelling Wastewater Magnetic materials |
Yayın Tarihi: | 15-Kas-2009 |
Yayıncı: | Wiley |
Atıf: | Uzun, L. vd. (2009). "Removal of heavy-metal ions by magnetic beads containing triazole chelating groups". Journal of Applied Polymer Science, 114(4), 2246-2253 |
Özet: | The aim of this study was to prepare magnetic beads that could be used for the removal of heavy-metal ions from synthetic solutions. Magnetic poly(ethylene glycol dimethacrylate-1-vinyl-1,2,4-triazole) [m-poly (EGDMA-VTAZ)] beads were produced by suspension polymerization in the presence of a magnetite Fe3O4 nanopowder. The specific surface area of the m-poly(EGDMAVTAZ) beads was 74.8 m(2)/g with a diameter range of 150-200 mu m, and the swelling ratio was 84%. The average Fe3O4 content of the resulting m-poly(EGDMA-VTAZ) beads was 14.8%. The maximum binding capacities of the m-poly (EGDMA-VTAZ) beads from aquous solution were 284.3 mg/g for Hg2+, 193.8 mg/g for Pb2+, 151.5 mg/g for Cu2+, 128.1 mg/g for Cd2+, and 99.4 mg/g for Zn2+. The affinity order on a mass basis was Hg2+ > Pb2+ > Cu2+ > Cd2+> Zn2+. The binding capacities from synthetic waste water were 178.1 mg/g for Hg2+, 132.4 mg/g for Pb2+, 83.5 mg/g for Cu2+, 54.1 mg/g for Cd2+, and 32.4 mg/g for Zn2+. The magnetic beads could be regenerated (up to ca. 97%) by a treatment with 0.1 M HNO3. These features make m-poly(EGDMA-VTAZ) beads potential supports for heavy-metal removal under a magnetic field. |
URI: | https://doi.org/10.1002/app.30511 https://onlinelibrary.wiley.com/doi/10.1002/app.30511 http://hdl.handle.net/11452/22853 |
ISSN: | 0021-8995 |
Koleksiyonlarda Görünür: | Web of Science |
Bu öğenin dosyaları:
Bu öğeyle ilişkili dosya bulunmamaktadır.
DSpace'deki bütün öğeler, aksi belirtilmedikçe, tüm hakları saklı tutulmak şartıyla telif hakkı ile korunmaktadır.