Please use this identifier to cite or link to this item:
http://hdl.handle.net/11452/25406
Title: | Growth and characterisation of electrodeposited Co/Cu superlattices |
Authors: | Kockar, Hakan Uludağ Üniversitesi/Fen-Edebiyat Fakültesi/Fizik Bölümü. Şafak, Mürşide Alper, Mürsel AAG-8795-2021 13613646100 7005719283 |
Keywords: | Co/Cu superlattices Electrodeposition Electrolyte pH Gmr Electrodeposition; Electrolytes Growth (materials) Magnetoresistance Polycrystalline materials Layer thicknesses Polycrystalline Titanium Superlattices Ni-cu/cu superlattices Giant magnetoresistance Composition dependence Multilayers Films Ni/cu Chemistry Science & technology - other topics Materials science Physics |
Issue Date: | Feb-2008 |
Publisher: | American Scientific Publishers |
Citation: | Şafak, M. vd. (2008). ''Growth and characterisation of electrodeposited Co/Cu superlattices''. Journal of Nanoscience and Nanotechnology, 8(2), 854-860. |
Abstract: | Ferromagnetic/non-ferromagnetic Co/Cu superlattices were grown on polycrystalline Titanium (Ti) W from a single electrolyte by electrodeposition. Microstructure and magnetoresistance (MR) of the superlattices were investigated as a function of the electrolyte pH as well as the layer thicknesses. Structural characterisation by X-ray diffraction (XRD) showed that the superlattices have face-centred cubic (fcc) structure with a strong (111) texture at the studied pH levels, but the texture degree is affected by the electrolyte pH. The scanning electron microscope (SEM) studies revealed that the superlattices grown at low pH (2.0) have smoother surfaces compared to those grown at high pH (3.0). The superlattices exhibited either anisotropic magneto resistance (AMR) or giant magnetoresistance (GMR) depending on the Cu layer thickness. The shape of MR curves changes depending on the combination of Co and Cu layer thicknesses. The superlattices with Co layers less than 3 nm and Cu layers less than 2 nm have broad and non-saturating curves, indicating the predominance of a superparamagnetic contribution, possibly due to the discontinuous nature of the ferromagnetic (Cc) layer. For superlattices with the same bilayer and total thicknesses, the GMR magnitude decreased as the electrolyte pH increased. Besides possible structural differences such as the texture degree and the surface roughness, this may arises from the variation in the Cu content of the ferromagnetic layers caused by the electrolyte pH. |
URI: | https://doi.org/10.1166/jnn.2008.B242 https://www.ingentaconnect.com/content/asp/jnn/2008/00000008/00000002/art00060 http://hdl.handle.net/11452/25406 |
ISSN: | 1533-4880 1533-4899 |
Appears in Collections: | PubMed Scopus Web of Science |
Files in This Item:
There are no files associated with this item.
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.