Başlık: | Properties of steel foundry electric arc furnace dust solidified/stabilized with Portland cement |
Yazarlar: | Uludağ Üniversitesi/Mühendislik Fakültesi/Çevre Mühendisliği Bölümü. Salihoğlu, Güray Pınarlı, Vedat Salihoğlu, Nezih Kamil Karaca, Gizem AAG-9399-2021 AAG-9413-2021 8551769300 8551769100 55665111200 8551769200 |
Anahtar kelimeler: | Dust stabilization Acid neutralization Cement Compressive strength Hazardous waste Industrial waste Landfill Leaching Sand Stabilization Steel Sand SPLP TCLP Leaching characteristics Setting time Silica Fume Stabilization Aggregate Wastes Lead Solidification/stabilization Performance Strength Environmental sciences & ecology |
Yayın Tarihi: | Eki-2007 |
Yayıncı: | Academic Press-Elsevier Science |
Atıf: | Salihoğlu, G. vd. (2007). "Properties of steel foundry electric arc furnace dust solidified/stabilized with Portland cement". Journal of Environmental Management, 85(1), 190-197. |
Özet: | Electric arc furnace dust from steel production is generated in considerable amounts worldwide and needs to be treated as hazardous waste. The aim of this study was to investigate the properties of electric arc furnace dust solidified/stabilized by using Portland cement. Mortar and paste samples were prepared with varying waste-to-binder ratios between 0% and 90%. A comprehensive experimental program was designed including XRF characterization, setting time, unconfined compressive strength, and toxicity characteristics leaching procedure (TCLP), synthetic precipitation leaching procedure (SPLP), and acid neutralization capacity (ANC) tests. The results were evaluated in order to determine if the solidified /stabilized product can be disposed of at a landfill site with domestic waste or at a segregated landfill. The effect of using sand on S/S performance was also investigated. The results indicated that the solidification /stabilization process using PC helps the heavy metals to be bound in the cement matrix, but the TCLP leaching results exceeded the EPA landfilling limits. The SPLP leaching results conformed to the limits implying that the waste or S/S products can be disposed of at a segregated landfill; however the low ANC of the S/S products reveals that there may be leaching in the long-term. The sand used in the mortar samples adversely affected the S/S performance, causing higher heavy metal leaching levels, and lower pH levels in the leachate after the TCLP extraction than those measured in the leachate of the paste samples. |
URI: | https://doi.org/10.1016/j.jenvman.2006.09.004 https://www.sciencedirect.com/science/article/pii/S0301479706002611 http://hdl.handle.net/11452/31696 |
ISSN: | 0301-4797 1095-8630 |
Koleksiyonlarda Görünür: | Scopus Web of Science |
Bu öğenin dosyaları:
Bu öğeyle ilişkili dosya bulunmamaktadır.
DSpace'deki bütün öğeler, aksi belirtilmedikçe, tüm hakları saklı tutulmak şartıyla telif hakkı ile korunmaktadır.